Dapre konpozisyon alyaj la epi itilize tanperati a, yo ka divize asye chalè ki reziste nan kategori sa yo:

Ba alyaj chalè ki reziste asye: sitou pa ajoute eleman alyaj tankou cr, mo, v, ti nan asye kabòn òdinè amelyore fòs la fluaj ak estabilite estriktirèl nan asye . Sa a ki kalite asye montre bon fòs ak severite nan tanperati ki wo ak se apwopriye pou divès jaden endistriyèl .}}}

Medium alloy heat-resistant steel: the main alloying element is Cr. With the increase of Cr content, high temperature resistance and oxidation resistance are enhanced. In order to improve creep strength and reduce temper brittleness, elements such as Mo are usually added. This type of steel performs well in medium and high temperature environments and is widely used in petrochemical and power Endistri .

High alloy heat-resistant steel: has high mechanical properties and oxidation resistance at temperatures above 600℃. According to its basic alloy system, it can be divided into chromium-nickel type and high chromium type. Elements such as Ti, Nb, Al, W, V, Mo, B, Si, Mn and Cu are often added to improve Pèfòmans . Sa a ki kalite asye se apwopriye pou anviwònman ekstrèm tanperati ki wo, tankou motè avyon ak réacteurs nikleyè .

‌Austenitic Chalè ki reziste Steel‌: Li se sitou ki konpoze de austenit-fòme eleman tankou nikèl, Manganèz, ak nitwojèn . Li gen bon severite, machin, ak weldability, epi li se apwopriye pou anviwònman wo-tanperati pi wo a 600 degre {{{5 {

‌Martensitic Chalè ki reziste Steel‌: kontni an CHROMIUM se jeneralman 7-13%. Li gen segondè-gwo tanperati fòs ak dlo vapè rezistans kowozyon anba a 650 degre, men pòv weldability‌ .

‌Ferritic Chalè ki reziste Steel‌: Li se moun rich nan CHROMIUM, aliminyòm, Silisyòm ak lòt eleman, fòme yon sèl-faz estrikti ferit, ak bon rezistans oksidasyon ak gwo tanperati gaz rezistans korozyon, men relativman ba gwo-tanperati fòs ak pòv weldability‌ .

‌Pearlite Chalè ki reziste Steel‌: Li se sitou ki konpoze de CHROMIUM ak MOLYBDENUM, ak kantite lajan an total jeneralman pa depase 5%. li gen bon-gwo tanperati fòs ak pèfòmans nan ranje tanperati a nan {{

Metòd sa yo klasifikasyon ede nou pi byen konprann karakteristik yo ki pèfòmans ak sijè ki abòde aplikasyon an nan chalè ki reziste asye nan senaryo aplikasyon diferan .